Cellular rubber

Joint découpé matière caoutchouc cellulaire 420x185

Joint découpé matière caoutchouc cellulaire 880 x 330

Cellular rubber for flat gaskets provides an optimal seal with minimal clamping force, thanks to its flexible cellular structure. It is the ideal solution for irregular or fragile surfaces.

Custom-cut cellular rubber flat gaskets

Our range of specialized materials meets all your requirements:
- EPDM & silicone: excellent thermal properties and UV resistance
- Neoprene & NBR: resistance to oils, hydrocarbons, and mechanical stress
- PE & EVA foams: lightweight solutions for cushioning and insulation

Suitable for gasket cutting, our products are manufactured according to your specifications, from prototypes to large-scale production runs.

Cellular rubber comparison chart for flat gasket cutting

Check out our cellular foam comparison chart:

Material code

Material type

Hardness
(Shore 00)

Density
(kg/m3)

Deformation
(%)

Compr. (%)

Water absorption
(%)

Constante T°  
(°C)
Peak T°
(°C)
Resistance Technical data sheet
EC001 CR 55 140 ± 30 25% (35-65 kPa)
50% (80-160 kPa)
*
< 25
< 5 -50 / +100 +110 Ozone
Abrasion
Atmospheric agent
Télécharger le PDF
CC001 EPDM 22 80 ± 20 25 (10-30 kPa)
50 (55-100 kPa)
*
< 30
< 5 - 50 / + 100 + 120   Télécharger le PDF
CC002 EPDM 35 120 ± 20 25 (13,8-62,1 kPa)
50 (80-160 kPa)

**
≤ 35


*** 
≤ 80

< 5 -40 / +100 +115 Ozone
Air
UV
Télécharger le PDF
CC003 EPDM 35 130 ± 20 25 (35-15 kPa)
50 (120-40 kPa)

**
≤ 25

< 5 -40 / +100 +120 Ozone
Corrosion
Tearing
Abrasion
Télécharger le PDF
CC004 EPDM 40 175 ± 25 25 (50-15 kPa)
50 (120-40 kPa)

**
< 25

< 5 -50 / +110 +120 Ozone
Abrasion
Bad weather
Télécharger le PDF
CC005 EPDM / 100 ± 20 25 (< 3 kPa)
50 (< 6 kPa)

**
<35

/ -50 / +100 + 120 Ozone
Air
UV
Télécharger le PDF
CC007 EPDM/CR 35 130 ± 25 25 (40 ± 15 kPa)
50 (120 ± 40 kPa)

**
< 25

< 5 -40 / +100 +120   Télécharger le PDF
SPEC1 EVA/PE 90 100 ± 25 /

**
< 6

< 5 -40 / +70 +80 Ozone
Abrasion
Bad weather
Télécharger le PDF
CC008 EPDM 45 100 ± 20 25 (30-60 kPa)
50 (80-120 kPa)
*
< 25
< 3 -30 / +85 -30 / +85 Ozone Télécharger le PDF
CC010 EPDM Peroxyde 35 100 ± 20 25 (30-60 kPa)
50 (80-160 kPa)
*
< 25
< 5 -30 / +60 +85 Ozone Télécharger le PDF
OVC01 NBR/PVC 50 180 ± 30 25 (30-50 kPa)
50 (80-160 kPa)

*
<35

< 5 -40 / +90 +110 Ozone
Abrasion
Bad weather
Télécharger le PDF
PEC01 PE 50 30 ± 4 25 (45-55 kPa)
50 (65-120 kPa)

*
<30

< 3 -40 / +80 / Ozone
Abrasion
Bad weather
Télécharger le PDF
FC001 Silicone 42 250 ± 20 40 (90 kPa)

****
< 12

< 5 -60 / +230 +250 Ozone
Oxidation
UV
Bad weather
Télécharger le PDF

* ISO 815-1, 23°C, 50%, 24h

** ASTM D1056, 23°C, 50%, after 24h

*** NFR 99-211, 40°C, 50%, after 22h

**** ISO 1856, 70°C, 50%, 22h

Do you need to cut flat cellular rubber gaskets?

From single units to large-scale production runs, we process cellular rubber according to your specifications. Our experts will help you select the right material for your industrial applications. Request a quote.

Only on request